- Highest R-value batt available in the market - R-49 ( 15” Thick)
- Easy one-step application
- Labor Savings
- Helps meet the New Energy Codes
- Eliminates the need to install multiple thickness of batts or additional loose fill installation for higher R-value specifications
Technical Data
R-value is determined using industry standard test method ASTM C 518 by accredited NVLAP testing facilities.ASTM C 665 requirements include the following test methods:
- ASTM C 518 and C 687 – Thermal Resistance (R-Value)
- ASTM E 84 – Surface Burning Characteristics
- ASTM E 970 – Critical Radiant Flux
- ASTM E 96 – Water Vapor Permeance
- ASTM C 553 – Moisture Absorption
- ASTM C 1304 – Odor Emission
- ASTM C 665 SECT 13.8 – Corrosiveness
- ASTM C 1338 – Fungi Resistance